Chesterton 800 GoldEnd® Tape

Category Polymer , Tape , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Chesterton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton 800 GoldEnd® Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chesterton® 800 GoldEnd® Tape is a high density moldable, dry PTFE thread sealing tape. It is a heavy duty, tear-resistant product containing more PTFE per inch than virtually any thread sealing tape on the market today. Chesterton 800 GoldEnd Tape is chemically inert and seals most types of threaded metal and plastic pipes and bolts. It is nonreactive with steam, water, air fuels, refrigerants, acids, alkalies, all solvents, and gases including hydrogen oxygen, ammonia, propane butane, and nitrogen. For nitric or mixed acid services, factory should be consulted. Chesterton 800 GoldEnd Tape is non-hardening and stays pliable without the breakage seen in other PTFE containing tapes. It places a slippery layer of PTFE between mated threads which remains flexible and resists vibration. Connections that might otherwise be destroyed are saved for reuse as tape eases disassembly. Slippage is minimized during application as deep penetration of threads is possible with the soft malleable tape. Joints can be adjusted 90° or more without a leak. Chesterton 800 GoldEnd Tape is packaged in rugged easy-to-carry spools which protect the tape from dirt and contamination. It is available in a variety of spool sizes and widths that can be easily carried in a tool case or tool belt.Features:UL Listed-US and CanadaMeets MIL-T-27730AConforms to FDA 21CFR 177.1615DVGW Approval NO. 96.01e907Acceptable for oxygen use.Non-aging. Non-hardeningHigh density, resists tearingChemically resistant, pH 0-14NSF H1, P1 - Registration number 134016Oxygen tested per ISO 10297 and ISO 11114-3 per Air LiquidBAM tested, Oxygen Cerfified to 100°C Bundesanstalt fuer material for schung. Ref. No. 11.1/46.513Benefits:Stays pliableAlways ready to useRequires fewer wrapsResists tearing and breakageWon't clog fuel linesApplications: Use Chesterton 800 GoldEnd Tape as a non-hardening, dry thread sealant for most liquids, gases, pneumatic and hydraulic fittings. Prevents bolts and fittings from seizing up to 260°C. Seals as plumbing and most industrial piping threadsInformation provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Thickness 90.0 microns
3.54 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.20 - 13.9 MPa
1190 - 2010 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Descriptive Properties Value Comments
Color Light Yellow
Pressure Testing 10000 psi
Fluids (Oils)
2503 psi
Gaseous Media (Nitrogen)
4350 psi
Liquid Oxygen
Users viewing this material also viewed the following: