Material Notes:
A 33% glass fiber reinforced, impact modified nylon 6 offering a combination of creep resistance, stiffness and toughness over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 145 MPa
21000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 203 MPa
29400 psi
ASTM D790
Flexural Modulus 6.90 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.85 J/cm
3.47 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Processing Properties Metric English Comments
Melt Temperature 254 °C
489 °F