Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carmel Olefins CAPILENE® TR 50 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® TR 50 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAPILENE® TR 50 is a medium melt flow rate heterophasic copolymer with very high impact strength, even at low temperature, designed for injection molding. This grade combines good processability and mechanical properties.Applications: CAPILENE® TR 50 is developed for injection molding of automotive parts, crates and pails.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
50 mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
50 mm/min; ASTM D638
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm

@Temperature -20.0 °C
1.87 ft-lb/in

@Temperature -4.00 °F
ASTM D256
6.00 J/cm

@Temperature 23.0 °C
11.2 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Vicat Softening Point 140 °C

@Load 1.02 kg
284 °F

@Load 2.25 lb
ASTM D1525
Users viewing this material also viewed the following: