Material Notes:
CAPILENE® R 50 is a polypropylene homopolymer intended for injection molding, characterized by good flow properties combined with good balance of stiffness and impact. APPLICATIONS CAPILENE ® R 50 is a general purpose homopolymer. Typical applications are household articles and garden furniture.
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.55 GPa
225 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm

@Temperature >=23.0 °C
0.562 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ASTM D648
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ASTM D1525