Material Notes:
40% Glass Reinforced, Impact Modified
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
dry; ISO 1183
Water Absorption 4.5 %
4.5 %
Sim. To ISO 62
Moisture Absorption 1.20 %
1.20 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 125 MPa
18100 psi
cond; ISO 527-1/-2
175 MPa
25400 psi
dry; ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
dry; ISO 527-1/-2
5.0 %
5.0 %
cond; ISO 527-1/-2
Tensile Modulus 7.50 GPa
1090 ksi
cond; ISO 527-1/-2
11.5 GPa
1670 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
9.50 J/cm²

@Temperature -30.0 °C
45.2 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eU
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eU
10.0 J/cm²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
cond; ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
cond; ISO 179/1eA
1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
dry; ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
dry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
dry; ISO 75-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
cond; IEC 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
cond; IEC 60093
Dielectric Constant 3.3

@Frequency 1.00e+6 Hz
3.3

@Frequency 1.00e+6 Hz
dry; IEC 60250
3.5

@Frequency 100 Hz
3.5

@Frequency 100 Hz
dry; IEC 60250
4.5

@Frequency 1.00e+6 Hz
4.5

@Frequency 1.00e+6 Hz
cond; IEC 60250
14

@Frequency 100 Hz
14

@Frequency 100 Hz
cond; IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
cond; IEC 60243-1
25.0 kV/mm
635 kV/in
dry; IEC 60243-1
Dissipation Factor 0.0090

@Frequency 100 Hz
0.0090

@Frequency 100 Hz
dry; IEC 60250
0.015

@Frequency 1.00e+6 Hz
0.015

@Frequency 1.00e+6 Hz
dry; IEC 60250
0.12

@Frequency 1.00e+6 Hz
0.12

@Frequency 1.00e+6 Hz
cond; IEC 60250
0.30

@Frequency 100 Hz
0.30

@Frequency 100 Hz
cond; IEC 60250
Comparative Tracking Index 600 V
600 V
cond; IEC 60112