Density 20.6 g/cc
0.744 lb/in³
Johnson Matthey FP Platinum w/ 3% Copper Jewelry Alloy
Soft for settings. Copper, cobalt, gold, iridium, palladium and ruthenium alloy easily with platinum. The differences between the alloys reflect the hardening of the alloying element itself.
Density 20.6 g/cc
0.744 lb/in³
Johnson Matthey SC 950 Platinum w/ 5% Palladium Jewelry Alloy
Castings, delicate settings. Palladium has been used to create casting alloys at various levels of fineness. Palladium produces a softer casting.
Density 20.6 g/cc
0.744 lb/in³
CMW® ELKONIUM 305 platinum based alloy
Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (..