Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 0.0000344 ohm-cm | <= 0.0000344 ohm-cm | 5% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 MH10, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Electrical Resistivity | <= 0.0000344 ohm-cm | <= 0.0000344 ohm-cm | 5% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 MH12, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Electrical Resistivity | <= 0.0000344 ohm-cm | <= 0.0000344 ohm-cm | 5% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 MH6, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Electrical Resistivity | <= 0.0000344 ohm-cm | <= 0.0000344 ohm-cm | 5% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 MH8, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Electrical Resistivity | <= 0.0000344 ohm-cm | <= 0.0000344 ohm-cm | 5% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 MH2, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Electrical Resistivity | <= 0.0000344 ohm-cm | <= 0.0000344 ohm-cm | 5% IACS conductivity (minimum) |
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Electrical Resistivity | 0.0000344 ohm-cm | 0.0000344 ohm-cm | 5 % IACS |
CMW® ELKONIUM 305 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Electrical Resistivity | 0.0000344 ohm-cm | 0.0000344 ohm-cm | 5 % IACS |
CMW® ELKONIUM 32 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |