Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 10.23 g/cc | 0.3696 lb/in³ | |
CMW® ELKONITE® G18 Molybdenum Silver contact material ASTM 662, Class B, infiltrated For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc. |