Material Notes:
Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyester compounds where consistent viscosity is critical and inherent low oil absorption provides higher filler loadings. Gel Talc and Body Filler talcs are platy, hydrophobic and non-abrasive.Body Filler talc is designed to allow the formulator to achieve maximum pigment/binder ratios.Information provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 2.78 g/cc
2.78 g/cc
Bulk Density 0.465 g/cc
0.0168 lb/in³
Loose
1.11 g/cc
0.0399 lb/in³
Tapped
Brightness 92 %
92 %
Hunter Y, Rd value, dry
Oil Absorption 24 %
24 %
g oil/100 g filler; ASTM D281
Fineness 2.0
2.0
Hegman Fineness; ASTM D1210
Moisture Absorption at Equilibrium <= 0.30 %
<= 0.30 %
Loss On Ignition 17 %
17 %
Particle Size 1.8 µm
1.8 µm
@ 10%
8.5 µm
8.5 µm
D50
30 µm
30 µm
@ 98%
pH 9.0
9.0
Mechanical Properties Metric English Comments
Hardness, Mohs 1.0
1.0
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
Component Elements Properties Metric English Comments
Al2O3 <= 1.0 %
<= 1.0 %
CaO <= 13 %
<= 13 %
Fe2O3 <= 1.0 %
<= 1.0 %
MgO 24 %
24 %
SiO2 46 %
46 %