Physical Properties Metric English Comments
Specific Gravity 2.78 g/cc
2.78 g/cc
Part A
Epoxy Technology EPO-TEK® E2001 Electrically Conductive, Silver-Filled Epoxy
Product Description: EPO-TEK® E2001 is a two component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications using a snap-cure profile. Advantages & Appl..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR Body Filler Talc for Polyester Filler
Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR CIMTUFF® 9102 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR CIMTUFF® 9103 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR CIMTUFF® 9103s Talc
CIMTUFF® 9103s talc is a treated talc produced from high purity ore, which provides low iron content, low surface area and superior color in dry form as well as when incorporated with resins. CIMT..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR CIMTUFF® 9107 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR CIMTUFF® 9110 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR CLEAR-BLOC® 80 Antiblock Talc
CLEAR-BLOC® 80 talc, produced from high purity ore provides high brightness, clarity, low iron content and low surface area for primary use as an anti-block additive in LDPE and LLDPE film applicat..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR FlexTalc® 1222 Ultrafine Talc for TPO Applications
Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR FlexTalc® 1222D Ultrafine Talc for TPO Applications, Densified
Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR FlexTalc® 610D Ultrafine Talc for TPO Applications, Densified
Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR Gel Talc for Polyester Filler
Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR MV 603 Talc
MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR MV 607 Talc
MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR RP 9305 Talc
RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR RP 9410 Talc
RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR FlexTalc® 610 Ultrafine Talc for TPO Applications
Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR FlexTalc® 815 Ultrafine Talc for TPO Applications
Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR FlexTalc® 815D Ultrafine Talc for TPO Applications, Densified
Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR MV 610 Talc
MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR RP 9310 Talc
RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R..
Specific Gravity 2.78 g/cc
2.78 g/cc
CIMBAR RP 9405 Talc
RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are..