Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.11 g/cc | 0.0399 lb/in³ | Tapped |
CIMBAR Body Filler Talc for Polyester Filler Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes.. |
|||
Bulk Density | 1.11 g/cc | 0.0399 lb/in³ | Tapped |
CIMBAR RP 9310 Talc RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R.. |