Material Notes:
Recovered polypropylene compositeInformation provided by Breplast S.p.A.
Physical Properties Metric English Comments
Density >= 0.900 g/cc
>= 0.0325 lb/in³
UNI EN ISO 1183-1
Melt Flow 9.0 - 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 - 10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.0 MPa
3770 psi
ISO 527
Tensile Strength, Yield 14.0 MPa
2030 psi
ISO 527
Elongation at Break 26 %
26 %
ISO 527
Flexural Strength 58.0 MPa
8410 psi
ISO 178
Flexural Modulus 0.950 GPa
138 ksi
ISO 178
Izod Impact, Notched 0.0900 J/cm
0.169 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 130 °C
266 °F
A50; ISO 306
Descriptive Properties Value Comments
Color Grey