Material Notes:
Daploy™ WB140HMS is a structurally isomeric modified propylene homopolymer. Applications: door liners, parcel shelves, microwaveable food packaging, cushioning and protective packaging, lightweight packaging trays, beakers and containers, technical foams for automotive applications such as headliners, carpet backing, thermal and acoustic insulation, thermoformable, foamed films and sheets, under the hood acoustic panels, and water shields.Information provided by Borealis AG
Physical Properties Metric English Comments
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527-2
Elongation at Yield 6.0 %
6.0 %
ISO 527-2
Tensile Modulus 2.00 GPa
290 ksi
ISO 527-2
Flexural Modulus 1.90 GPa
276 ksi
2mm/min; ISO 178
Charpy Impact, Notched 0.100 J/cm²

@Temperature -30.0 °C
0.476 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-2