Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Blue River Coatings Steel Seal Primer

Category Polymer , Adhesive , Thermoset
Manufacturer Blue River Coatings
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Blue River Coatings Steel Seal Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BLUE RIVER COATINGS STEEL SEAL PRIMER is a high quality, single component primer, not requiring any catalyzing agent. STEEL SEAL PRIMER is designed for dip coaters who need a quick, fast drying paint for corrosion resistance and high gloss. STEEL SEAL PRIMER dries in about 6-8 minutes @ 70°F and 50% humidity. STEEL SEAL PRIMER offers good coverage and durability, as well as being a low VOC and EPA compliant coating. Enviromental Advantages:BLUE RIVER COATINGS STEEL SEAL PRIMER is a low VOC (Volatile Organic Compound), high performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling. Characteristics: Excellent dip coatingGood hardness/impact resistanceGood mar and abrasion resistanceSolvent resistantCan be applied in a wide variety of temperature and humidity conditions without the use of retarders Distilled water is used for reductionWater is used for clean-upNon-Hazardous80% gloss on 60° glossometerAir dry or force curing preferredCan be oven bakedWide range of colorsCoating will not flash rust on bare metalShelf life of 1 yearUnused paint can be returned to containerNon-FlammableUsesSteelAluminumMetal Pipe Salt Fog in Harshaw No. 22 cabinet via ASTM B117 procedures with 5% NaCl solution. Evaluation of panels follows ASTM D610, D714, and D1654.200 hoursScribed – 1/16” dense #4. Moderate rust rundown OK – moderate rust rundownUnscribed – OK – moderate rust rundownInformation provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Density 1.03 g/cc
0.0372 lb/in³
Solids Content 32 %
32 %
by volume
35 %
35 %
by weight
Volatile Organic Compounds (VOC) Content 60 g/l
60 g/l
pH 7.0 - 8.5
7.0 - 8.5
Mechanical Properties Metric English Comments
Impact Test 11.3 J
8.33 ft-lb
Reverse/direct on steel
Thermal Properties Metric English Comments
Boiling Point 169 °C
336 °F
Flash Point 65.6 °C
150 °F
Processing Properties Metric English Comments
Cure Time 1.00 min

@Temperature 75.0 °C
0.0167 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
4.02 min

@Temperature 75.0 °C
0.0670 hour

@Temperature 167 °F
Dust Free, at 50% humidity
4.02 - 4.98 min

@Temperature 75.0 °C
0.0670 - 0.0830 hour

@Temperature 167 °F
Recoat, at 50% humidity
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Evaporation Rate Slower than ether
Theoretical Coverage 514 ft2 at 1 mil
Vapor Density Heavier than air