Bisalloy Steels BisPlate 450 Thickness 8-20 mm

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel , Carbon Steel , Low Carbon Steel
Manufacturer Bisalloy Steels
Trade Name BisPlate
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bisalloy Steels BisPlate 450 Thickness 8-20 mm.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A through hardened, abrasion resistant steel plate, with guaranteed high impact toughnessApplications: Dump Truck Bodies, Mining Buckets, Tipper Bodies, Cutting Edges, Dump Truck Wear Liners, Construction Waste Bins, Liner Plates/ChutesTesting: AS/NZS 1816, AS/NZS 1544Tolerance: In accordance with AS/NZS 1365
Mechanical Properties Metric English Comments
Hardness, Brinell 425 - 475
425 - 475
Tensile Strength at Break 1400 MPa
203000 psi
Tensile Strength, Yield 1150 MPa

@Strain 0.200 %
167000 psi

@Strain 0.200 %
Elongation at Break 12 %
12 %
in 50 mm GL
Charpy Impact 17.0 - 25.0 J

@Temperature -40.0 °C
12.5 - 18.4 ft-lb

@Temperature -40.0 °F
Longitudinal
Component Elements Properties Metric English Comments
Boron, B 0.0020 %
0.0020 %
Carbon, C 0.23 %
0.23 %
Chromium, Cr 0.90 %
0.90 %
Iron, Fe 97.7 %
97.7 %
As Balance
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 0.15 %
0.15 %
Phosphorous, P 0.025 %
0.025 %
Silicon, Si 0.60 %
0.60 %
Sulfur, S 0.0050 %
0.0050 %
Descriptive Properties Value Comments
CE (IIW) 0.45
CET 0.35
Surface Finish Shotblasted