Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 1150 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1150 MPa

@Strain 0.200 %
167000 psi

@Strain 0.200 %
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 1150 - 1300 MPa

@Strain 0.200 %
167000 - 189000 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 1400 DP High-strength Steel
The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel ..
Tensile Strength, Yield 1150 MPa

@Strain 0.200 %
167000 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 450 Thickness 8-20 mm
A through hardened, abrasion resistant steel plate, with guaranteed high impact toughnessApplications: Dump Truck Bodies, Mining Buckets, Tipper Bodies, Cutting Edges, Dump Truck Wear Liners, Constr..
Copyright © lookpolymers.com All Rights Reserved