Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 17.0 - 25.0 J @Temperature -40.0 °C |
12.5 - 18.4 ft-lb @Temperature -40.0 °F |
Longitudinal |
Bisalloy Steels BisPlate 450 Thickness 8-20 mm A through hardened, abrasion resistant steel plate, with guaranteed high impact toughnessApplications: Dump Truck Bodies, Mining Buckets, Tipper Bodies, Cutting Edges, Dump Truck Wear Liners, Constr.. |
|||
Charpy Impact | 16.9 J | 12.5 ft-lb | V-Notch; Air Cooled from 941°C; 200°C Temper Temperature |
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7) TLS S7 Shock-Resisting tool steel is an air or oil hardening tool steel that is characterized by very high impact toughness. The combination of strength and high toughness makes S7 tool steel a cand.. |