Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBATRON C1065X1 PPS, cross-linked, 65% glass fiber / mineral reinforced

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Manufacturer Barlog Plastics
Trade Name KEBATRON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBATRON C1065X1 PPS, cross-linked, 65% glass fiber / mineral reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPS-GF/MD 65Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.94 g/cc
0.0701 lb/in³
ISO 1183
Water Absorption 0.020 %
0.020 %
similar to ISO 62 test
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527-1
Elongation at Break 1.0 %
1.0 %
ISO 527-1
Tensile Modulus 19.0 GPa
2760 ksi
ISO 527-1
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
Melting Point 285 °C
545 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL Registered; IEC 60695-11-10
Descriptive Properties Value Comments
Resin Type PPS-GF/MD 65
Users viewing this material also viewed the following: