Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 285 °C | 545 °F | |
Omnia Plastica PPS GF40 Polyphenylenesulphide Crystalline polymer based on polyphenylene sulfide with the addition of 40% glass-fibre. Very high rigidity, stiffness and flexural strength. The temperature resistance is very high: up to 240° C. .. |
|||
Melting Point | 285 °C | 545 °F | |
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Melting Point | 285 °C | 545 °F | |
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Melting Point | 285 °C | 545 °F | Average value: 285 °C Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Melting Point | 285 °C | 545 °F | ISO 11357-3 |
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
Melting Point | 285 °C | 545 °F | ISO 11357-3 |
Solvay Specialty Polymers Ryton® QC200N Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
Melting Point | 285 °C | 545 °F | ISO 11357-3 |
Solvay Specialty Polymers Ryton® QC220N Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON C1040G5 PPS, cross-linked, 40% glass fiber reinforced PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON C2040G5 PPS, cross-linked, 40% GF, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON C2065X3 PPS, cross-linked, 65% glass fiber / mineral reinforced, reduced residual chlorine PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON L1040G3 PPS, linear, 40% glass fiber reinforced PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON L1065X3 PPS, linear, 65% glass fiber / mineral reinforced PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON L2040G3 PPS, linear, 40% glass fiber reinforced, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | DIN 53765 |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Melting Point | 285 °C | 545 °F | |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Melting Point | 285 °C | 545 °F | |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |