Material Notes:
TPC-ETInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
Tensile Strength at Break >= 15.0 MPa
>= 2180 psi
ISO 527-1
Elongation at Break >= 600 %
>= 600 %
ISO 527-1
Charpy Impact, Notched NB
NB
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Resin Type TPC-ET