Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 4042 Polypropylene, Fiber/Filament Grade

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 4042 Polypropylene, Fiber/Filament Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene PP4042 is a fiber extrusion resin with excellent thermal and mechanical properties. This product meets FDA standards for food contact applications.Applications: Rope and twine, fibrillated tape, slit film.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
D-1505
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
2 in/min; D-638
Elongation at Yield 10 %
10 %
2 in/min; D-638
Flexural Modulus 1.25 GPa
182 ksi
D-790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
D-648
Descriptive Properties Value Comments
Process Fiber
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved