Bapolan® PS6078-G Polystyrene Compound

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Bapolan®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolan® PS6078-G Polystyrene Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolan 6078-G is a colored, high impact polystyrene.Applications: General purpose.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers. All data is based on molded plaques.
Physical Properties Metric English Comments
Melt Flow 8.0 g/10 min
8.0 g/10 min
200'C/5,000g; ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D-638
Flexural Modulus, 1% Secant 2068 MPa
299900 psi
ASTM D-790A
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D-256
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
International