Material Notes:
Description: Ultramid A3L HP UV BK23220 is an unreinforced, impact modified, UV stabilized, high flow nylon 66 for injection molding. This grade has excellent flow and improved ambient and low temperature toughness.Applications: Cable ties, fasteners and clamps.Information provided by BASF