Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Master Builders Solutions ChemRex® CX Concrete Floor Primer - Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer BASF Master Builders Solutions
Trade Name ChemRex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Master Builders Solutions ChemRex® CX Concrete Floor Primer - Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CX Concrete Floor Primer is a waterborne epoxy primer for concrete substrates. It is designed to manage and reduce moisture vapor emission (out-gassing) of concrete slabs by controlling the rate of transmission through the permeance of the primer.CX Concrete Floor primer is used on concrete floors and slabs, interior use, where low-odor applications are desired, where moisture vapor transmission of substrate exceeds 3 lb./1060 sq. ft./24 hours, and where vapor drive of porous concrete surfaces needs to be controlled.The percent solid content is 51%. The drying time is 5 hours. The flash point is >200° given the ASTM D 93 test conditions. The VOC content is 118 g/L (0.99 lbs./gallon). The pull off strength after a 7 day cure is >300, depending on substrate. The coverage rate is 350-400 sq. ft. per gallon.After one week CX Concrete Floor Primer is resistant to phosphoric acid (5%), acetic acid (5%), lactic acid (10%), diesel, motor oil, hydrogen peroxide, and salt water. After one week it is not resistant to nitric acid (5%), hydrochloric acid (10%), Sulfuric acid (10%), jet fuel, gasoline, and brake fluid. Information provided by ChemRex, Inc.Product of former ChemRex, Inc. BASF launched the Master Builders Solutions brand on January 15, 2014.
Physical Properties Metric English Comments
Viscosity Measurement 260
260
Mechanical Properties Metric English Comments
Taber Abrasion, mg/1000 Cycles 43
43
1000 g load (after a 7 day cure); ASTM D 4060-90
Optical Properties Metric English Comments
Gloss 62 %
62 %
at 60° angle; TTS-141C method 6101.1
Processing Properties Metric English Comments
Processing Temperature 20.0 °C
68.0 °F
Pot Life 90 min
90 min
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved