Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Luwax® OA 5 Pastilles/Powder

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer BASF
Trade Name Luwax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Luwax® OA 5 Pastilles/Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Oxidized polyethylene wax with high hardness and a low acid number. Important applications include emulsion for coating citrus fruit, paper, cellophane, textiles and flooring.Information provided by BASF
Physical Properties Metric English Comments
Viscosity Measurement 350 - 470

@Temperature 120 °C
350 - 470

@Temperature 248 °F
[mm<sup>2<sup>/s], Melt; DGF M-III 8
Mechanical Properties Metric English Comments
Ball Indentation Hardness 450 MPa
65300 psi
DGF M-III 9a
Chemical Properties Metric English Comments
Total Acid Number 15 - 19
15 - 19
[mg KOH/g]; DGF M-IV 2
Descriptive Properties Value Comments
Color Off-White
Congealing Point 98°C
DGF M-III 3
Copyright © lookpolymers.com All Rights Reserved