Mechanical Properties Metric English Comments
Ball Indentation Hardness 450 MPa
65300 psi
H 961/30; ISO 2039/P1
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures  (disconti
Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application ..
Ball Indentation Hardness 450 MPa
65300 psi
DGF M-III 9a
BASF Luwax® OA 5 Pastilles/Powder
Description: Oxidized polyethylene wax with high hardness and a low acid number. Important applications include emulsion for coating citrus fruit, paper, cellophane, textiles and flooring.Informatio..
Ball Indentation Hardness 450 MPa
65300 psi
H 961/30; ISO 2039/P1
Hexion Bakelite™ PF 7595 Phenolic Formaldehyde Resin, Low Coefficient of Friction, Galvanized, Conductive  (di
Phenolic molding compound, inorganically/organically filled, modified with graphite, good heat conductivity, good sliding properties, conductive in electrical properties.Application areas: Bearers f..