BASF Basantol® 273 Orange Liquid

Category Fluid
Manufacturer BASF
Trade Name Basantol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Basantol® 273 Orange Liquid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Structure: Azo/1:2 Cr-ComplexColour Index: Acid Orange 142Application: Dye for wood stainsPhysical Form: LiquidInformation provided by BASF
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Descriptive Properties Value Comments
Color Orange
Composition Dye Content
0.22