Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Owens Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for use with strong alkalis. Data provided by the manufacturer, Owens Corning.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
24 hrs.; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 68
68
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
ASTM D638
Modulus of Elasticity 15.7 GPa
2280 ksi
ASTM D638
Flexural Strength 310 MPa
45000 psi
ASTM D790
Flexural Modulus 10.0 GPa
1450 ksi
ASTM D790
Compressive Strength 220 MPa
31900 psi
ASTM D695
Izod Impact, Notched 10.4 J/cm
19.5 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 16.9 µm/m-°C

@Temperature 20.0 °C
9.40 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.26 J/g-°C
0.300 BTU/lb-°F
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
ASTM D648
Flammability, UL94 V-0
V-0
5V
Electrical Properties Metric English Comments
Dielectric Constant 4.4

@Frequency 60 Hz
4.4

@Frequency 60 Hz
ASTM D150
Arc Resistance 188 sec
188 sec
ASTM D495