Material Notes:
Soft, general purpose, highly filled extrusion compound recommended for cove base moldings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.46 - 1.50 g/cc
1.46 - 1.50 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78
72 - 78
delayed; ASTM D-2240
Tensile Strength, Yield 9.65 MPa
1400 psi
ASTM D-638
Elongation at Yield 350 %
350 %
ASTM D-638
100% Modulus 0.00503 GPa
0.730 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 166 °C
330 °F