Polymer Property : 100% Modulus = 0.00503 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00503 GPa
0.730 ksi
ASTM D412
Mearthane Durethaneâ„¢ S DS-685A Solid Polyurethane Elastomer
MDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
100% Modulus 0.00503 GPa
0.730 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00503 GPa
0.730 ksi
ASTM D-638
Axiall 8757 Moldings & Extrusions Flexible PVC
Soft, general purpose, highly filled extrusion compound recommended for cove base moldings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00503 GPa
0.730 ksi
ASTM D-638
Axiall 10705 Wire & Cable Flexible PVC
Non-lead stabilized general purpose 75C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf..
100% Modulus 0.00503 GPa
0.730 ksi
ASTM D-638
Axiall 10706 Wire & Cable Flexible PVC
Non-lead stabilized 80C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall C..
100% Modulus 0.00503 GPa
0.730 ksi
ASTM D-638
Axiall 10702 Wire & Cable Flexible PVC
General purpose 80°C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..