Axiall 835WA Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 835WA Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AWM for SPT, SJT and SVT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.37 g/cc
1.33 - 1.37 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 86
80 - 86
delayed; ASTM D-2240
86 - 92
86 - 92
ASTM D-2240
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D-638
Elongation at Yield 291.1 %
291.1 %
Air Aging: 7 days @ 113°C; 75-mil plaques; UL 1581
355 %
355 %
ASTM D-638
100% Modulus 0.00965 GPa
1.40 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D-746
Oxygen Index 23 %
23 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F