Axiall 36431 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 36431 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
80°C rated, semi-rigid insulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.34 g/cc
1.30 - 1.34 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 50 - 56
50 - 56
delayed; ASTM D-2240
61 - 67
61 - 67
ASTM D-2240
Tensile Strength, Yield 25.9 MPa
3750 psi
ASTM D-638
Elongation at Yield 250 %
250 %
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -21.0 °C
-5.80 °F
ASTM D-746
Oxygen Index 30 %
30 %
ASTM D-638
Electrical Properties Metric English Comments
Dielectric Constant 3.9

@Frequency 1000 Hz
3.9

@Frequency 1000 Hz
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F