Material Notes:
Non-lead stabilized, 720 hour sunlight resistant, TW insulation compound also recommended for 75C Class 43 applications or outdoor jacket applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.39 - 1.43 g/cc
1.39 - 1.43 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 79 - 85
79 - 85
delayed; ASTM D-2240
Tensile Strength, Yield 15.9 MPa
2300 psi
ASTM D-638
Elongation at Yield 350 %
350 %
ASTM D-638
100% Modulus 0.008791 GPa
1.275 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D-746
Oxygen Index 25 %
25 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F