Polymer Property : 100% Modulus = 0.008791 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.008791 GPa
1.275 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.008791 GPa
1.275 ksi
ASTM D-638
Axiall 13820 Wire & Cable Flexible PVC
Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications. Good low temperature performance. Also suitable for outdoor jacket applicatio..
100% Modulus 0.008791 GPa
1.275 ksi
ASTM D-638
Axiall 13821 Wire & Cable Flexible PVC
Non-lead stabilized, 720 hour sunlight resistant, TW insulation compound also recommended for 75C Class 43 applications or outdoor jacket applications.Information provided by Georgia GulfGeorgia Gul..
100% Modulus 0.008791 GPa
1.275 ksi
ASTM D-638
Axiall 8810 Moldings & Extrusions Flexible PVC
Low gravity extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required. Exhibits good flex whitening resistance.Information pro..
100% Modulus 0.008791 GPa
1.275 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..