Polymer Property : Volume Resistivity = 6.00e+14 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
STN 34 6460
Plastcom SLOVAMID® 6 GF 65/2M PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 65% of glass fiber, for moldings used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby to..
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
ASTM D257
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
Momentive Performance Materials RTV118 One Component Acetoxy Adhesive Sealant, Translucent
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Volume Resistivity >= 6.00e+14 ohm-cm
>= 6.00e+14 ohm-cm
ASTM D 257
Karina 951-35/4-IS-LMP Ivory PVC Compound
Heavy metal free PVC compound with high electrical insulation resistance. Recommended for insulation of CI and CCI cables.Information provided by Karina Indústria e Comércio de Plásticos Lt..
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
Momentive Performance Materials TSE3940 Flame Retardant Adhesive Sealant, Gray
TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater..
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
ASTM D257
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
IEC 60093
Polyplastics Duranex® 6300T Polybutylene Terephthalate (PBT), Low friction, Low wear, Mineral filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
Tra-Con Tra-Bond 723C01 One-Part Medical Grade Adhesive
TRA-BOND 723C01 is a fast, heat curing, one component adhesive targeted at medical applications. The material complies with USP Class VI toxicity requirements and is resistant to gamma sterilization..
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
Dow Corning HV 1540/20P BASE AND CLEAR CURING AGENT
32 Shore, very low viscosity, castable hydrophobic silicone rubber with high tear strength and low temperature cure.Information provided by Dow Corning
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
Dow Corning SLYGARD® 535 THIXOTROPIC DIELECTRIC GEL
Information provided by Dow Corning
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
dry; IEC 60093
DSM Novamid® 1010GN2-30 NAT/BK37 PA6-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
dry; IEC 60093
DSM Novamid® 1013G15 1 NA PA6-GF15
15% Glass Reinforced, Injection Molding
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
dry; IEC 60093
DSM Novamid® 1013GH15 1 NA/BK37 PA6-GF15
15% Glass Reinforced, Heat Stabilized, Injection Molding
Volume Resistivity <= 6.00e+14 ohm-cm
<= 6.00e+14 ohm-cm
Cytec (Conap) FR-1272 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Volume Resistivity >= 6.00e+14 ohm-cm
>= 6.00e+14 ohm-cm
ASTM D257
Fainplast Compounds Hax™ HFX 505/2 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Com..
Volume Resistivity 6.00e+14 ohm-cm

@Temperature 20.0 °C
6.00e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257
Fainplast Compounds HAX HF 4221 Halogen Free PVC
General purpose
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
50% RH; ASTM D-257
Axiall 13821 Wire & Cable Flexible PVC
Non-lead stabilized, 720 hour sunlight resistant, TW insulation compound also recommended for 75C Class 43 applications or outdoor jacket applications.Information provided by Georgia GulfGeorgia Gul..
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
ASTM D257
Fainplast Compounds Hax™ HF 213 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:General purpose, improved processabilityInformation provided by Fainplast Compounds
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
Conditioned; ASTM D257
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..