Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 859 Nylon 6, Pellet form

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 859 Nylon 6, Pellet form.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ashlene 859 is offered in small pellet form. It is dried to less than 0.1% moisture eliminating the need for predrying. Ashlene 859 is molded with wall thickness ranging from 1/16" to greater than 1".Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.8 %
1.8 %
ASTM D570
Mechanical Properties Metric English Comments
Elongation at Yield 100 %
100 %
ASTM D638
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
351 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
ASTM D648
Users viewing this material also viewed the following: