Material Notes:
Nylon 6 resin for blown or caste film, in addition to co-extrusion applications.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.6 %
1.6 %
24 hrs; ASTM D570
Moisture Absorption at Equilibrium 2.7 %
2.7 %
50% RH; ASTM D570
Water Absorption at Saturation 9.5 %
9.5 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.0 MPa
8700 psi
ATSM D638
Elongation at Break 290 %
290 %
ASTM D638
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418