Ashley Polymers Ashlene® 1503WO BK Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, UV Stabilized
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 1503WO BK Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A rigid flame retardant polycarbonate, UV stabilized in black for applications requiring superior dimensional stability and overall toughness.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM D785
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ATSM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 3.30 GPa
479 ksi
ASTM D790
Izod Impact, Notched 0.990 J/cm
1.85 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
286 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in