Material Notes:
Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa Parts, Impellers, Valve Bodies, Electrical Base Pans, Fuse Box Components, Control Boxes, Electrical Boxes, Battery CasesInformation provided by Asahi Kasei
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
23°C
Filler Content 20 %
20 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 94.0 MPa
13600 psi
Flexural Modulus 4.85 GPa
703 ksi
Izod Impact, Notched 0.980 J/cm
1.84 ft-lb/in
ASTM 3.2mm
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 139 °C
282 °F
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
50% RH