Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 23.0 - 105 µm/m-°C | 12.8 - 58.3 µin/in-°F | Average value: 77.6 µm/m-°C Grade Count:12 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
CTE, linear, Transverse to Flow | 23.0 µm/m-°C | 12.8 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings |
|||
CTE, linear, Transverse to Flow | 23.0 µm/m-°C | 12.8 µin/in-°F | z direction |
Arlon TC350 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |