Material Notes:
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
Silicone Property; Arlon SQA-TMS-024
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 5.55 MPa
805 psi
Silicone Property; ASTM D412
Tensile Strength, Yield 6.03 MPa

@Strain <=1.00 %
875 psi

@Strain <=1.00 %
Silicone Property; Arlon-SAQ-TMS-008
Elongation at Break 400 %
400 %
Silicone Property; ASTM D412
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Modulus 0.00201 GPa
0.292 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C

@Temperature 20.0 - 160 °C
100 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Specific Heat Capacity 1.14 J/g-°C

@Temperature 100 °C
0.272 BTU/lb-°F

@Temperature 212 °F
Silicone Property; E1461-01
Thermal Conductivity 0.400 W/m-K

@Temperature 100 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg -117 °C
-179 °F
Silicone Property; ASTM D3418
Electrical Properties Metric English Comments
Dielectric Constant 3.4

@Frequency 1.00e+6 Hz
3.4

@Frequency 1.00e+6 Hz
D<sub>k</sub>, Silicone Property; IPC TM 650-2.5.5.3
Dissipation Factor 0.0050

@Frequency 1.00e+6 Hz
0.0050

@Frequency 1.00e+6 Hz
D<sub>f</sub>, Silicone Property; IPC TM 650-2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 121 °C
0.250 hour

@Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 7.22 °C
6.00 Month

@Temperature 45.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Light Blue
Plasticity 2.02 mm
Arlon SQA-TMS-005