Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.03 MPa | 875 psi | ASTM D412 |
Polymax® Maxelast® P1945 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 6.03 MPa @Strain <=1.00 % |
875 psi @Strain <=1.00 % |
Silicone Property; Arlon-SAQ-TMS-008 |
Arlon CP-499CA Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |