Material Notes:
OREVAC 18729 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18729 is an extrusion adhesive to be used in coextrusion technologies. As adhesive, OREVAC 18729 has been designed to develop adhesion between PP and EVOH or PP and PA.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Index of Compound 4.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.0 MPa
5950 psi
ASTM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 615 %
615 %
ASTM D638
Flexural Modulus 0.750 GPa
109 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 162 °C
324 °F
DSC
Vicat Softening Point 137 °C
279 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 230 °C
446 °F
Adapter Temperature 230 °C
446 °F
Die Temperature 230 °C
446 °F
Users viewing this material also viewed the following: