Polymer Property : Adapter Temperature = 230 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 230 °C
446 °F
Average value: 230 °C Grade Count:4
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Adapter Temperature 230 - 250 °C
446 - 482 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1068D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 230 - 250 °C
446 - 482 °F
Extrusion Molding
LG Chemical KEYFLEX BT 2140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 230 - 250 °C
446 - 482 °F
Extrusion Molding
LG Chemical KEYFLEX BT HB9255D Ester Type TPE
Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical
Adapter Temperature 230 - 240 °C
446 - 464 °F
Extrusion
Kolon DIAMAT® EG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Adapter Temperature 230 - 240 °C
446 - 464 °F
Extrusion
Kolon DIAMAT® EH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Adapter Temperature 230 - 240 °C
446 - 464 °F
Extrusion
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Adapter Temperature 230 - 240 °C
446 - 464 °F
Extrusion
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Adapter Temperature 230 - 240 °C
446 - 464 °F
Extrusion
Kolon DIAMAT® IG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Adapter Temperature 230 - 240 °C
446 - 464 °F
Extrusion
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Adapter Temperature 230 - 240 °C
446 - 464 °F
Extrusion
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Adapter Temperature 230 °C
446 °F
Arkema Group OREVAC® 18360 Maleic Anhydride Modified Polyethylene
OREVAC® 18360 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1..
Adapter Temperature 230 °C
446 °F
Arkema Group OREVAC® 18370 Maleic Anhydride Modified Polyethylene
OREVAC® 18370 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1..
Adapter Temperature 230 °C
446 °F
Arkema Group OREVAC® 18380 Maleic Anhydride Modified Polyethylene
OREVAC® 18380 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1..
Adapter Temperature 230 °C
446 °F
Arkema Group OREVAC® 18707 Grafted Maleic Anhydride Polypropylene
OREVAC 18707 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18707 ..
Adapter Temperature 230 °C
446 °F
Arkema Group OREVAC® 18722 Maleic Anhydride Modified Polypropylene
OREVAC 18722 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18722 ..
Adapter Temperature 230 °C
446 °F
Arkema Group OREVAC® 18729 Grafted Maleic Anhydride Polypropylene
OREVAC 18729 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18729 ..
Adapter Temperature 230 °C
446 °F
Arkema Group OREVAC® 18365 Maleic Anhydride Modified Polyethylene
OREVAC® 18365 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1..
Adapter Temperature 230 - 240 °C
446 - 464 °F
Average value: 235 °C Grade Count:3
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Adapter Temperature 230 - 240 °C
446 - 464 °F
Extrusion Molding
LG Chemical KEYFLEX BT S5035 Ester Type TPE
Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide..