Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Film Grade
Manufacturer Arkema
Trade Name LOTRYL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LOTRYL® 24 MA 005 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 24 MA 005 is a polymer of choice for applications where softness, flexibility and polarity are required. Typical applications are flexible film, polyesters modification and cable compounds.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Methyl Acrylate Content 23 - 26 %
23 - 26 %
IRTF (internal)
Melt Index of Compound 0.40 - 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 - 0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 750 %
750 %
ASTM D638
Flexural Modulus 0.0180 GPa
2.61 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 72.0 °C
162 °F
DSC
Vicat Softening Point 45.0 °C

@Load 1.02 kg
113 °F

@Load 2.25 lb
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F