Thermal Properties Metric English Comments
Vicat Softening Point 45.0 °C

@Load 1.00 kg
113 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding
Greenflex HN 70 is an ethylene vinyl acetate copolymer (EVA) for compounding applications. Greenflex HN 70 is a medium fluidity grade with high tack.Main Applications: Greenflex HN 70 is recommend..
Vicat Softening Point 45.0 °C
113 °F
ASTM D1525
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced  (discontinued **)
Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: Flame Retardant: Balance of Properties (Impact, Mechanical and Heat)Applications: Computer, Monitor and Printer Housings, Microwave Co..
Vicat Softening Point 45.0 °C
113 °F
50 N; ISO 306
Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding
Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is f..
Vicat Softening Point 45.0 °C
113 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
DuPont Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer
Elvaloy® 3427 AC can be used for coextrusion and compounding. It can also be used in extrusion coating. Elvaloy® 3427 AC is very soft and flexible, and has good adhesion to various polymers. It..
Vicat Softening Point 45.0 °C
113 °F
ASTM D1525
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low..
Vicat Softening Point 45.0 °C
113 °F
ISO 306/A
ExxonMobil EXACT™ 8210 Plastomer for Multilayer Film Applications
Product Description: Exact 8210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications req..
Vicat Softening Point 45.0 °C
113 °F
Rate B, ASTM D1525-70
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium
Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Vicat Softening Point 45.0 °C
113 °F
Rate B, ASTM D1525-70
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium
Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions ..
Vicat Softening Point 45.0 °C
113 °F
ASTM D1525
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate
OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low ..
Vicat Softening Point <= 45.0 °C
<= 113 °F
ASTM D1525
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer
AFFINITY™ EG 8150G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene alpha-olefin copolymer exhibiting high flexibility and elasticity. It can be ut..
Vicat Softening Point <= 45.0 °C
<= 113 °F
ASTM D1525
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
AFFINITY™ EG 8200G Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. It exhibits high flexibility and elasticity. It can be utilized in monolayer cast film and in ..
Vicat Softening Point 45.0 °C

@Load 1.02 kg
113 °F

@Load 2.25 lb
ASTM D1525
Arkema Group LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 24 MA 005 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 24 MA 005 is a poly..
Vicat Softening Point 45.0 °C

@Load 0.999 kg
113 °F

@Load 2.20 lb
ASTM D1525
Arkema Group LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3430 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3430 is a versatile adhesive for extrusion coating or lam..
Vicat Softening Point 45.0 °C

@Load 0.999 kg
113 °F

@Load 2.20 lb
ASTM D1525
Arkema Group LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4403 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER 4403 is a versatile adhesive for extrusion lamination, de..
Vicat Softening Point 45.0 °C

@Load 0.999 kg
113 °F

@Load 2.20 lb
ASTM D1525
Arkema Group LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4503 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process.LOTADER 4503 is a versatile adhesive for extrusion lamination, des..
Vicat Softening Point 45.0 °C

@Load 0.999 kg
113 °F

@Load 2.20 lb
ASTM D1525
Arkema Group LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 5500 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. These grade is characterised by a high fluidity. Functional group..
Vicat Softening Point 45.0 °C
113 °F
ASTM D1525
Westlake EMAC® SP2261 23% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2261 is a 23% EMA copolymer containing antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal tempe..
Vicat Softening Point 45.0 °C
113 °F
B (50N); ISO 306
Borealis Daplen™ EE103AE TPO Compound
Daplen EE103AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE103AE is a material with excellent impact /stiffness ratio. Thanks to its low ..
Vicat Softening Point 45.0 - 95.0 °C
113 - 203 °F
Average value: 73.0 °C Grade Count:13
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m..
Vicat Softening Point 45.0 °C
113 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer  (discontinued **)