Aremco Pyro-Tape™ 682-AR High Temperature Tape Single-layer ultra-high molecular weight polyethylene with a rubber adhesive

Category Polymer , Adhesive , Tape
Manufacturer Aremco
Trade Name Pyro-Tape™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Pyro-Tape™ 682-AR High Temperature Tape Single-layer ultra-high molecular weight polyethylene with a rubber adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications Abrasion Resistance Features Low coefficient of friction to reduce wear, scratching and noise. Liners for chutes, rails and slides.
Physical Properties Metric English Comments
Thickness 229 microns
9.00 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.207 MPa

@Thickness 25.4 mm
30.0 psi

@Thickness 1.00 in
Adhesive Bond Strength 0.0302 MPa

@Thickness 25.4 mm
4.38 psi

@Thickness 1.00 in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 2.3
2.3
Dielectric Strength 591 kV/mm
15000 kV/in