Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® N110L (Dry) Nylon 6, 10% Glass Fiber Reinforced, Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N110L (Dry) Nylon 6, 10% Glass Fiber Reinforced, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: LubricatedForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Filler Content 10 %
10 %
Water Absorption 1.5 %
1.5 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 4.96 GPa
720 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
395 °F
Unannealed; ASTM D648