Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 3320 HVAC Construction

Category Metal , Nonferrous Metal , Aluminum Alloy , Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 3320 HVAC Construction.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aluminum foil/scrim/laminate. UL 723 Classified.Information provided by 3M
Physical Properties Metric English Comments
Thickness 152 microns
6.00 mil
Backing; ASTM D3652
170 microns
6.70 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.9 MPa
6080 psi
ASTM D3759
Peel Strength 0.88746 kN/m
5.0625 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 79.0 °C
174 °F
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic
Users viewing this material also viewed the following: