Material Notes:
Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencies..Advantages: The Speed grades provide an excellent compromise between mechanical properties and lossesApplications: Speed has been developed for very high speed rotors. This enables manufacturers to make more compact machines for a given mechanical outputRecommendations for use: Speed grades can be used immediately after lamination punching. The effect of punching can be eliminated if a stress relief annealing is applied. This optimises the performance of the Speed grades in applications with fine teeth. It can also provide substantial performance improvements in the lower frequency range. To achieve these effects, a C5 type coating is advised. Speed stacks can be produced using any existing assembly technique such as interlocking or welding.Information provided by ArcelorMittal
Physical Properties Metric English Comments
Density 7.60 g/cc
0.275 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 210 - 240
210 - 240
L direction
210 - 240
210 - 240
T direction
Tensile Strength, Ultimate 570 - 620 MPa
82700 - 89900 psi
L direction
590 - 640 MPa
85600 - 92800 psi
T direction
Tensile Strength, Yield 440 - 490 MPa
63800 - 71100 psi
L direction
485 - 515 MPa
70300 - 74700 psi
T direction
Elongation at Break 20 - 30 %
20 - 30 %
L direction
20 - 30 %
20 - 30 %
T direction
Magnetic Properties Metric English Comments
Core Loss <= 23.0 W/kg

@Frequency 400 Hz
<= 10.4 W/lb

@Frequency 400 Hz
at 1T, Guaranteed
<= 60.0 W/kg

@Frequency 700 Hz
<= 27.2 W/lb

@Frequency 700 Hz
at 1T, Indicative
Descriptive Properties Value Comments
Anisotropy >15%
400 Hz at 1T
Polarization >1.51 T
at 2,500 A/m
>1.62 T
at 5,000 A/m
>1.72 T
at 10,000 A/m
Users viewing this material also viewed the following: